Default Yellow NiteMare is Over It's DONE !!!! :)

Well here is it folks no more Orange. The frame is done in 2 parts
Caswell's Bright White and another suppliers Fluorescent Yellow. Problem came in when the other folks supplied the WRONG Cure temps and time sheet.. The right times and temps are 392 Degrees for 7 mins not 15 mins or 325 degrees for 10 mins. Hmm the sheet I received said 400 Degrees for 15 mins, Problem was it was burning the yellow and turning it Orange...

The color is Hard to photograph as well as apply
Want to thank everyone again for all the Help..
Thanks folks...