Any ideas on this problem would be appreciated...here are the details:
3.6 sq.in surface area to coat on ID
7.2 A
12V car battery with charger
Resistance with bulbs in parallel
3 hours plating time
surface cleaned very well and water break tested
The result is very little plating. I have plated sample parts to test the batch and have good results, but cannot get ID setup to work. Please click this link if you want to see pictures. Click on the pictures for a larger view.
http://home.earthlink.net/~sc.co/