Welcome to our forum Jasonboulanger.

To start, read the recent thread "New to Anodizing", Scockin provides a link to download the LCD instructions. Do this first, the answers to nearly all of your questions are there.

Regarding your power supply.
Sorry, it won't work without extensive internal electronic modifications, these don't have any means to control the current, which is absolutely necessary for successful anodizing. The LCD instructions detail a method to hook up an ordinary 600W lamp dimmer to the AC side of an automotive battery charger, so that the current can be controlled by varying the voltage. This method will not work with your power supply, don't try it.