Default Lolipop Blue

Had the chance today to try one of my new colors which is the lolipop blue. This is a transparent color. In the three pics posted, there is no base, just bare metal after it was glass beaded. O a nieghbor kid wanted me to "try" this new color to his bike pegs.. After this now he wants his bike done the same way.. Also if Caswell likes the pics Ill gladly take another pound of lolipop blue.. of course.....

http://www.caswellplating.com/bbs/al...php?pic_id=319
http://www.caswellplating.com/bbs/al...php?pic_id=318
http://www.caswellplating.com/bbs/al...php?pic_id=317