Our supplier specifies this heat as optimum.
NAPA acid = prod # 9002 Try any battery supplier.

Sealing in the dye isn't in the procedure. You could try it - but don't complain if it doesn't work.

Airbrushing will result in the possibility of a weaker color. You may need to increase the concentration to counter this.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote