I did some more Copy Chrome today. I took more time. Seems to be better, thicker.
I also tried Silver Brush Plating on brass today. I was using the 4.5 volts in the Copy Chrome kit. I also heated the brass in warm water prior to plating.
I did about 3 sq inches for 15-20 minutes. I obtained a black-ish layer, which I was expecting. When I went to polish it with Flitz, it all came off.
Do I need lower voltage or what?
|