Default Type III (hard coating)?

I have read on may sites that Type III anodizing is very hard to do (most small shops use type II).

The only notes I seem to see repeatedly: current density is much higher and temperature is much lower.

If these are the only differences between type II and type III, I should be able to overcome this.

I have ac and dc welders capable of 300 amps. Low temperatures can be obtained by using dry ice.

Is there something I am missing

Also, I read about the LCD kit. Is this process true type III or just a good type II process?

Thanks .... Mike