Just ordered the Blue 4A dye from the UK Caswell distributor

Cant wait, Andodizing tank is setup, will be using 10% Sulphuric Acid (due to not being able to find battery acid!). As my electrolyte.

I really need to find a CC Rectifier I think, battery charger just wont cut it.

Will let you know how I get on.

The Ally is all the same, sheet stuff, it is olted together to make a box.....(ECU Case), so I am hoping to get the same blue on all the peices, fingers crossed. If Anodizied and Dyed for the same amount of time it should be!