Default Bronzing Baby Shoes

I was using a spray sealer, rather than soaking. But most likely it would not have made much of a difference, as the coating peeled on solid objects such as glazed ceramics and seashells, which indicates a problem with the copper spray coating and not the base sealer or lack therof.

The copper spray coating is solvent based from Caswell, a product, which I have been led to believe, has been discontinued. (Why ?)

In the meantime, my Canadian Caswell rep, Jim McMillen, has agreed to forward me some Silvaspray at cost minus what I had paid for the copper conductive paint. A very good and highly appreciated customer support tactic I must say.

Hopefully I will have better results to report back on later. I will keep you informed.

Thanks for the prompt customer feedback. And thanks Jim for your loyal support.