Default how do i tell if something is anodized?

I am polishing car wheels and am 50/50 for sure if the lip is anodized. I am thinking about just trying to polish the wheel, and if it doesnt work, then the lip is anodized.
I tried to test conductivity, and I get intermittent results.

Lets say, if a solid bar is anodized, will it be conductive?
Are there easier ways to tell if something is anodized?