yes it works , I've done it few times not on complicated art though
you need to use high temp ceramic paint
the one used for porcelain ceramic crafts and that needs to be baked at 350 degress
YOU CAN"T GO HIGGER THAN 350
I cure the clear for 15 mins at 350 it's a bit under the recuired time for curing but It worked fine.
I used paint n' bake paint found it at a local craft store.
|