View Single Post
  #1 (permalink)  
Old 01-16-2005, 09:25 PM
broker1234 broker1234 is offline
Newbie
 
Join Date: Jan 2005
Posts: 2
broker1234
Default stripping anodizing off aluminum

Hi Guys,
I'm planning to polish a bunch of airplane parts that currently have a brushed finished, covered with some sort of clear anodizing. I'd like to strip this off and polish out the aluminum. I have some polishing experience from my hot rod days years ago, so I consider myself just knowledegable to be dangerous...

I know I can sand the finish off, but this is time/labor intensive and will leave a rougher finish to polish out. I have also tried oven cleaner and it appears to work, but the underlying aluminum seems to be pitted and rough. At this time the only polishing stuff I have is one small dremel wheel, so I can't even tell for sure...

Any suggestions??? I'm going to order a polishing kit from Caswell, and want to get all I need!