i see what you are saying . well i have the titanium heaters coming from process tech. hope they solve my problem. we have burnt out 6 1000 wat titaniums so far by way of condensation over the tank with the lids . getting kinda expensive. the ones we ordered are 305 a peice so with any luck we will solve this problem. thanks for the feed back. clydes