Thread
:
keeping my shine?
View Single Post
#
2
(
permalink
)
01-19-2005, 09:47 AM
scocklin
Newbie
Join Date: Nov 2004
Location: Newburg, MD
Posts: 48
I pre-wash in simple green solution and warm water. Then dip in hot cleaner, but I keep the temp at about 150 degrees. Spray the part with distilled water to further knock any compound off make sure it passes the water break test.
scocklin
View Public Profile
Send a private message to scocklin
Find all posts by scocklin