View Single Post
  #3 (permalink)  
Old 11-08-2002, 09:32 AM
KevinW KevinW is offline
Newbie
 
Join Date: Nov 2002
Location: NJ
Posts: 2
KevinW
Default

Thanks! Flash Copper and copychrome it is.

One final clarification.

Once I acid dip to remove the chrome, will I still need to "activate" the nickel prior to the flash copper coat?

NEW TOPIC

I was also reading about the Flash copper over Pot Metal. It looks like Flash copper will do the job for copy chroming the pot metal.

Looks like clean, de-pit and dip the PM to clean off the coats, flash copper, fill pits, flash copper again, then Copy chrome.

This sounds like a much easier procedure on PM then the PM primer, or solder-it paste. Am I correct? I would like to do this on outside door handles. Thanks, Kevin