That is what I am trying to find out, ARE there differances with the copy chrome and what they are, good or bad.

My long range goal is to try and build a plating busisness, because there is nothing like that anywhere around my area, and I think it could be a thriving busisness. I realize that every busisness has it's pitfalls, but if some of these problems could be avoided by using the copy chrome it would sure make it easier to get something going. But if I am comparing apples to oranges then thats a whole different story.

Let me ask it another way, if I copper plated then nickel plated two identical items , then chromed one and copy chromed the other and they both came out perfect , how much of a differance would there be between them, color shine , durability etc.