Well, after performing about 20 dummy plating sessions with the copper-ized bath.... everything still comes out copper plated (yes, the polarity is correct this time). I must have really slammed that solution. All the copper is off the nickel plates, but for the life of me I cannot seem to clear the bath. Looks like a Caswell order is in my future...

- Mark