I have done allot of items that had been polished. I just did a dozen oval brass sailboat window frames. The customer was sick of polishing them every week only to have them oxidize again & again. The brass did darken a little when cured.
Just make sure you use a pre paint prep to clean off any old wax or polish.
Good Luck