first,i have friends who have tried clearcoating after polishing(even clear powder coating)but it doesn't hold up.then you have to strip it off and re-polish again.as far as stripping it off,it depends on the piece.i usually try to stip it chemically (paint&decal remover type stuff)or use a d-a type sander w/320 or400 grit paper.if the part is anodized,u can use ez off oven cleaner to get down to bare metal.then polish hard w/tripoli and finish with green or white rouge.hope it helps