View Single Post
  #3 (permalink)  
Old 11-21-2002, 12:33 PM
Sunshine Sunshine is offline
Newbie
 
Join Date: Nov 2002
Posts: 2
Sunshine
Default

I've been told that the base metal is steel and that the clear coat can be removed and then the brass plating buffed lightly. The clear coat would then need to be reapplied. The pitting is down to the metal.

Thanks