the powder booth is just a device to contain the powder dust, I hang stuff from the rafters if need be, the booth just gives you better control over the goodies floating around in the air and sure makes clean up alot easier.. I prefer to ground to the part, but i have rods that i hang from and if im doing multiple parts i just grund to the rod.