I could not go into a larger tank mainly due to size and the amount of chemicals needed. My work area is shrinking as I get more into this hobby. The tank is tall so I'm going to try several pieces at a time at various depths. The use of aluminum bars sounds like a good idea. Would two or three bars running the length of the tank spaced evenly around the tank work?