Ive been having bad results at the moment with silvaspray, though i reckon a great part of the prob is that my parts are very hard to wire up correctly for decent current flow, but brush painted results have been awful. Seems the brushstrokes affect the way the silver particles settle and cause uneven plating.
Ive found you will need to up the plating times considerably to get a decent deposit.
Anone on here had good results with silvaspray? did you use longer plating times/higher current?