I built an oven a little smaller than yours, 36CF, and I heat it with 4ea 3000 watt elements. It heats up to 450 in less than 10 minutes. You may need a little more wattage. I figure mine does well with 333watts per CF.
Take a look at it at
www.powdercoatoven.4t.com
Gary