Spiral wheels with black compound should be able to do the job. You can also try the greaseless compound, which is more aggressive than the black emery.

Have you tried something like a nylon brush? See http://www.caswellplating.com/nbb350.htm
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote