thank you for your reply. I just tried a 4" sewn cotton wheel with a green bar last night and it worked pretty good. I have sanded the heads to 400 grit then started with the 4" wheel. I will try the black tonight my customer was here last night when I tried the wheel and he was happy with the outcome

I do a lot of OEM factory wheels with clear coat and machine lines. What would you recommend for buffing wheels for these I have been using Zephyr air way buffs (orange,green, and white) I use paint remover to get the clear off then size permiting i use an electric da sander to sand the maching lines