04-06-2005, 09:42 AM
R-Wells
Newbie
Join Date: Mar 2005
Posts: 32
I cant really say, since I dont really know what peak voltage would have been for sure.
At 90 minutes I was at 11.3 volts.
The parts I did Monday I ran for 120 minutes peaked at 11.5v. and decreased to 11.4
Thanks
Rusty
R-Wells