I posted a couple of pic's of some cast aluminum parts off my motorcycle. Not exactly large projects, but you gotta start some where, right? I've also been working on the exhaust cans I will post a few pic's of them soon. I don't think I was overloading the wheels, they have stayed nice and fluffy since the start. Not enough pressure to melt the compound. One thing I've noticed with both the stainless and aluminum parts that are round (tubular shaped) is buffing lengthwise looks much better than if I were to buff around them. Not sure if that's the correct method, but it's working for me. My thinking was to buff around the part to avoid any flat spots. Thanks for the advice.