Well, I guess I will let go a little longer then.

I usullay checked the part after about 10 minutes. Powder always was 'flowing' by then.

Thanks for the tips.

The one piece that I had to recoat because it fell off the hook in the oven... it sure seemed to cure nice. Took a LOT more blasting to get the coating off than it took to get the paint off.