Lot's of money, the chemicals are extremely expensive. Electropolish is basically used as a final surface prep for a micron fine finish for use in steril enviroments. You can't just take some ugly scatched up peice and put it in and majically have a mirror finish, you still have to do the initial prep the old fashioned way.
|