i know what you mean my rig runs at about 9000sfm w/ 10" wheels and i get great results. i dont know if you have tried vented wheels but it seems to work better for me the regular spiral wheels, they seem to hold up to more pressure and last longer. keep us posted on the results of the new motor
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
|