Hey, I actually bought the Caswell Anodize stipper for 50 bucks...and all it is is SODIUM HYDROXIDE...go to ebay and search for it. For about 4 dollar plus shipping you can get like 3 times the amount. BE CAREFUL with it!!! It's super corrosive!