hey dude,,,pickleboy is right on the money,,,I woul start with
1.Heavy acid wash
2.Sand with orbital starting at 120,or 150 grit ,working your way up to 400,,minimum
3.hardest treated wheel to start with the brown bar,,,then loose white wheel,,with white compound,and they should turn out like glass