that is going to be extremely difficult, but not impossible. start off with cartridge rolls or cratex wheels. you will have to search for them as caswells does not sell them yet. they come in many shapes and sizes and used w/ a dremel. this will get the smoothing done. as for shine most of your polishing will be done whith loose wheels. order some just for that job as you will use loose w/ black, brown, as well as white so the buff can get between the fins. it is a lot slower this way but works. or try to find real narrow sewn and sisal wheels. i just remembered that there is a knife making company out of oklahoma that sell thin buffs. try internet search for knife building supplies. it starts with a j. all i can say here i dont want to anger the host. as always best of luck and post pics so we can all see bro.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
|