Default

I use one of these whenever I'm working on an area that has tight radii or sharp edges that need to maintain a square or flat profile. You can also relax with this tool a little bit and not worry about getting a wavy surface (very easily) from using round bits on an area that is long and flat.





Hope that helps.


-Rob-