View Single Post
  #2 (permalink)  
Old 05-15-2005, 10:57 PM
sswee's Avatar
sswee sswee is offline
Moderator
 
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,229
sswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the rough
Default

It appears to be a poor mix in the cast. I've had similar problems with some automotive parts. I plan to strip, repolish and anodize without using the DeOx/DeSmut to see if thats what is causing the problem to show so bad. Was the marker polished originally or matte finish?