I can't say for sure on the black oxide coating working with the high temps of brake rotors but I would think it would be alright. I can tell you for sure that black is the preferred color for heat dissappation and you'll need to either mask off the pad swept area or have a skim cut on the rotors after coating. If you black oxide your rotors, be sure to let us know the end results.