zincate on aluminum
This is my first try at plating aluminum with bright nickel (electro). Ordered Zincate solution and mixed according to the manual. Waterbreak showed fine. Question: Should the zincate solution dry completely before going into the nickel bath? Or should I rinse with distilled water before going in to rinse off the excess zincate?
The part starts reacting immediately to the zincate so I left it in about 30 sec. This part was mirror polished when it went in and came out of the zincate a dull grey. Will I still get a bright finish when nickeled? Any advice would be greatly appreciated.
|