I have had a hell of a time with spraying a clear, I am doing 2 different colors on a part and wanted to clear it so the tape line cant be felt. I applied the 1st color and flowed it, then the 2nd color of course masking the area before applying the powder and flowed it. After 20 min at 350-400 I removed the part and allowed the part to cool down some what and sprayed the clear on, it started flowing immediately in some areas, but in others it never did flow not even after reheating the part to 350-400 for 20 min. Whats the deal? This clear is a pain in da rear!!! I restripped the part today