Quote:
|
Originally Posted by berndog
any ideas how I can get into nooks and crannies?I'm using electric handheld polisher & air die grinder
|
on the small parts i do, i have found that for starters a felt bob in the die grinder w/ greasless works wonders. the bob are in all kinds of shapes so you should be able to find one that works for most tight spots. once you get done, you can also use the bobs for compound. the only caution i can give is load the bobs slowly or they will get overloaded and not work. best of luck bro.
ps: remember the pics so we can admire please.