Keep getting blisters in flash copper plating...HELP
I am new at this. I sanded and prepped the part. Cleaned it in sp degreaser then distilled water. Then I zincated the aluminum part...let it drip dry then went into the flash copper.
After plating there are small blisters that I can pop and peel. Why is this happening. Also after nickel plating the flash copper it is not shiny. When I did the practice copper pieces in the nickel it looked like chrome. I just cant get past the flash copper stage. All the parts that I am doing are aluminum.
|