I have a 40lb floor blaster , 60gal compresor and a blasting 4x3x4 cabinet
I use glassbeads for powder coating and silica or aluminum oxide for ceramic coatings
but most of the time I just send the part to be blasted for $10 and I don't have to deal with it.
|