Default So far not so good stripping chrome.

Ok...here goes. All the plating was removed no problem inside the valve cover however, on the outside surface, where rust was present, the acid bath did do considerable damage to the base metal. It's a good thing this was a "test" exercise. I'd hate to do that on good parts. Anyway, practice makes perfect.