Copy Chrome??
I just tried to chrome the front brackets that hold my floorboards
on my Bike the steel is 3/8 inch thick with 1/8 inch smaller steel
bracket welded to it had in the bucket for over an hour in a half
only the edges were chromed what am I doing wrong?? After I tried
them I tried a smaller peice and it worked great.
|