I tend to use black on sisal then black on one of caswell's finger buffs (orange or soft) and it comes up a treat

ALso those finger buffs are very thin and get into corners nicely as they 'crush' down a bit. Brown dosn't really do much after that so I go over with white on a nice soft loose wheel.