Sounds like under cure to me too. I have had luck with rebaking to the cure specs and was able to eliminate all the little cracks. Mostly happens to clear coat.........but seeing how candy colors are largely made up of clear I can see it happening with them to.Try a hard rebake.Let us know what happens.