Well i tryed a few types of tape today. Below is the rating.(no pics my camera in in the car )

1. Green fiber glass tape : Perfect little glue from curing
2. 3m Painters tape : Nightmare stuck like cement on block took 3 hours to remove.
3. white fiber glass cloth.. : Perfect but not cheap

well to remove the cheaper 3m painters tape ( blue ) you need to get a spray bottle and put light cuts in it. then spray it down few sprays. i get it wet and wait a few minutes then spray it again. and it comes right off then a little thinner to clean it up.

Now when you got a big part ( wheel)
Foil or the white fiber glass cloth.

I will get a few pics of this so what i am getting at DON'T try to cut corners it just give you more work and less time showing you perfect part off