THE 'RESIST' YOU NEED
You can use Clear Lacquer to protect areas of parts you do not want to plate.
It can be left on after plating or removed with Lacquer Thinner.
If you're going to plate with Copper...leave the 'resist' on it since you'll need to spray a coating of Clear Lacuer on the finished plating anyway to prevent it from oxydizing.