If you try a 3m type of disk it will help with the swirls, go to maxtools.com and look at their grinding disk they have the sand paper disk and the 3m disk get the med. and course 3m disk and then try your white, or blue rouge with a loose cotton wheel on a 7"or 9" grinder.
|