chrome is funny to coat over some times .. Some times i can shoot the candy and trans with no problems by blasting it defeats the purpose of candy coating... But when it comes to straight top coating i powder right over it no blasting at all 2 coats of base ... mirror and high glass only get 1 then a coat of clear will come next..
|